Skip to main content
dryadopen

Effect of Nd on high temperatures deformation and corrosion behavior of AZE Mg alloy

<p>An extruded AZE Mg alloy (Mg-3Al-1Zn-0.6Nd) has been developed and prepared to examine the effect of the precipitated phase on corrosion and hot deformation behavior. High-temperature compression experiments show that dynamic recrystallization (DRX) occurs at various experimental parameters (473 to 673 K and 1×10<sup>-4</sup> s<sup>-1</sup> to 1×10<sup>-3</sup> s<sup>-1</sup>). The deformation mechanism is dominated by dislocation slip and/or twinning. Al<sub>11</sub>Nd<sub>3</sub> precipitates with two different sizes could impede nucleation and the growth of DRXed grains. Serrated flow occurred owing to the interactions between dislocations and precipitates. The corrosion current density decreases with the addition of Nd elements. Moreover, the continuous precipitation of the Al<sub>11</sub>Nd<sub>3</sub> phase at grain boundaries reduces the corrosion rate in NaCl solution, thereby enhancing the corrosion resistance of AZE alloys.</p>

ShareScore

40/100

Overall dataset sharing score

Score breakdown

These five areas show where the dataset supports — or may limit — practical reuse.

Stewardship
4
Harmonization
12
Access
12
Reuse readiness
0
Engagement
12

Topics