Quasi-static tensile properties of PMMA (Elium 188) and Epoxy (Epopox A-28) resins
<p>The quasi-static tensile properties of PMMA (Elium 188) and Epoxy (Epopox A-28) resins are summarised in Table 1. <br> </p> <ul> </ul> <table> <caption>Table 1. The average tensile properties of epoxy (Epopox A-28) and PMMA (Elium 188) resins</caption> <tbody> <tr> <td>Property</td> <td>Epoxy</td> <td> PMMA</td> </tr> <tr> <td>Young's modulus of elasticity (GPa)</td> <td>2.3 <span class="math-tex">\(± \)</span> 0.1</td> <td>2.6 <span class="math-tex">\(± \)</span> 0.1</td> </tr> <tr> <td>Tensile failure strength (MPa)</td> <td>53.7 <span class="math-tex">\(± \)</span> 1.1</td> <td>63.5 <span class="math-tex">\(± \)</span> 0.3</td> </tr> <tr> <td>Elongation at failure (%)</td> <td>6.1 <span class="math-tex">\(± \)</span> 0.4</td> <td>6.6 <span class="math-tex">\(± \)</span> 0.3</td> </tr> </tbody> </table> <p> </p> <p><strong>Summary of the materials</strong>:</p> <ul> <li>The epoxy was a standard resin (Epopox A-28, Amroy Europe, Lahti, Finland) polymerised by a polyether diamine hardener (Jeffamine D-23, Hunstman, Texas, USA) with a 35 wt% hardener to epoxy ratio. The resin was degassed before casting into an aluminium-made mould. The resin was cured following the manufacturer's instructions (i: at 90 °C for 24 h. ii: 150 °C for 2 h). The Epopox A-28 was used as an alternative for EPON 828 epoxy resin.</li> <li>The PMMA was in-situ polymerised at the ambient conditions by mixing a liquid methyl methacrylate thermoplastic resin (Elium 188, Arkema, Colombes, France) and dibenzoyl peroxide initiator (BP-50-FT1, United Initiators GmbH, Pullach, Germany) with 3 wt% initiators to resin ratio. The resin was degassed before casting into an aluminium-made mould. </li> </ul> <p><strong>Summary of the tensile testing</strong></p> <p>The quasi-static tensile tests were performed using a universal testing machine (model 5967, Instron, MA, USA). The testing was performed according to the ISO 527 testing standard. The dimensions of the dog-bone shape coupons were 4 mm (thickness) <span class="math-tex">\(× \)</span> 10 mm (width) <span class="math-tex">\(× \)</span> 170 mm (full-length). The gauge length was 50 mm. The specimen was prepared as 1A type in ISO 527. <br> The tensile tests were performed by 30 kN load cell and 2 mm/min displacement rate. The displacement was recorded by a clip-on extensometer.</p>
ShareScore
32/100
Overall dataset sharing score
Score breakdown
These five areas show where the dataset supports — or may limit — practical reuse.
- Stewardship
- 4
- Harmonization
- 4
- Access
- 16
- Reuse readiness
- 8
- Engagement
- 0
Dataset details
- Repository
- zenodo
- Published
- November 29, 2022
- License
- cc-by-4.0
- DOI
- 10.5281/zenodo.7381443
Scored with release 0.9.0
ScienceDex for faculty
Your academic CV and NIH biosketch
Make your CV in your school's format and your NIH biosketch from it, then download both as Word files.